来源:http://www.jnjgcg.com/ 日期:2021-01-26 发布人:
复合板厂家说筒体为复合板制作的塔器,经常会遇到塔内件支撑件是焊在复合板的基层,还是焊在覆层的问题。
The manufacturer of clad plate said that for the tower made of clad plate, the problem of whether the support parts of tower internals are welded on the base of clad plate or on the cladding is often encountered.
如果焊在覆层,除了校核内件支撑件与覆层连接焊缝的强度,还应考虑基层和覆层的结合强度。而要求焊在基层的,多半是担心基层和覆层的结合强度。
If it is welded on the cladding, in addition to checking the strength of the connection weld between the internal support and the cladding, the bonding strength between the base and the cladding should also be considered. And the requirements of welding in the base, mostly worried about the bonding strength of the base and cladding.
内件支撑件焊在基层的难点,在于需要小心翼翼地剥开覆层,而不能伤害基层。
The difficulty of welding the internal support in the base course is to peel off the cladding carefully without damaging the base course.
另外,如果内件支撑件(如锆材)不能与基层(如碳钢)焊接,那也只能焊在覆层了。(锆材是不能与碳钢或不锈钢进行熔化焊的)
In addition, if the internal support (such as zirconium) can not be welded with the base (such as carbon steel), it can only be welded in the cladding. (zirconium materials cannot be fusion welded with carbon steel or stainless steel)
对于制造单位来说,要求内件支撑件焊在复合板制筒体的基层上,困难在于剔除复层加工槽的难度很大,必须严格控制加工精度,否则容易伤及基层材料,并且不可避免地会延长工期,和增加成本。
For manufacturing units, it is difficult to require the support parts of internal parts to be welded on the base of composite plate cylinder, because it is very difficult to remove the multi-layer processing groove. The processing accuracy must be strictly controlled, otherwise it is easy to damage the base material, and will inevitably extend the construction period and increase the cost.
一般情况下,复合板结合剪切强度都高于焊缝金属许用剪切应力,也就是说,内件支撑件与覆层的连接焊缝即使被拉裂了,复层结合强度也不会被破坏。
In general, the bonding shear strength of clad plate is higher than the allowable shear stress of weld metal, that is to say, the bonding strength of clad plate will not be damaged even if the connecting weld between the inner support and cladding is cracked.
但对于钛、锆等材料许用应力比较低的情况,上述校核也是有可能不合格的,此时可通过调整焊缝形式来增强其承载能力。
However, when the allowable stress of titanium, zirconium and other materials is relatively low, the above check may also be unqualified. At this time, the bearing capacity can be enhanced by adjusting the weld form.
复合板厂家说随着我国复合板爆炸技术水平的提高,复层结合强度已能满足内件支撑件焊缝强度的需求。所以在内件支撑件与筒体连接焊缝强度计算合格的前提下,从设备制造难度、制造工期及经济成本等因素综合考虑,内件支撑件宜直接焊接在复合板筒体的复层上。
The manufacturer of clad plate said that with the improvement of explosion technology level of clad plate in China, the bonding strength of clad plate has been able to meet the requirement of weld strength of internals support. Therefore, on the premise that the strength calculation of the welding seam between the inner support and the cylinder is qualified, the inner support should be directly welded on the cladding of the composite plate cylinder considering the difficulty of equipment manufacturing, manufacturing period and economic cost.
下一篇:彩钢板在冬季的保养方法 上一篇:影响C型钢被腐蚀的因素!
此文关键词: 济南复合板厂
阅读/ Recommended reading
- 济南彩钢板:屋顶太吵怎么办?坚固彩钢来帮助! 2024-11-21
- 济南复合板厂:复合板对人体有危害吗? 2024-11-20
- 济南彩钢板:哪种颜色更耐晒? 2024-11-18
- 济南彩钢板:彩钢板上做防水材料那种比较好? 2024-11-16
济南复合板厂:质量问题莫担忧
[2018-08-23]
复合板的质量通常取决于其制造材料和工艺。以下是一些关于复合板质量的信息: The quality of composite panels usually depends o...